ScanningTunnelingMicroscopy Chromium Phthalocyanine SmallScan Temasek_Lab Styrene thermal_property SetpointMode Galfenol 2dMaterials IndiumTinOxide LiftHeight DNA PinpointPFM LFM gallium_nitride Hexylthiophene Sphere ConductingPolymer Protein Dental Nanostructure ElectroChemical Aluminum rubber Electical&Electronics IIT-chennai NUS_Physics NiFe BlockCopolymer MultiLayerCeramicCapacitor DataStorage Adhesive Forevision PvdfFilm
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Block copolymer Ι
Scanning Conditions
- System: NX20
- Scan Mode: Tapping
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 0.8Hz
- Pixel: 512×512
- Scan Mode: Tapping
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 0.8Hz
- Pixel: 512×512