Fe-Nd-B Alloy

Fe-Nd-B Alloy

Scanning Conditions

- System: NX10
- Scan Mode: MFM
- Cantilever: PPP-MFMR (k=2.8N/m, f=75kHz)
- Scan Size: 15μm×15μm
- Scan Rate: 0.5Hz
- Pixel Size: 512 × 256
- Lift height: 100nm