PS/LPDE

PS LDPE

Spincast layer of PS/LDPE blend on Si. Signal change by thermal conductivity difference.

Scanning Conditions

- System: NX10
- Scan Mode: SThM
- Cantilever: NanoThermal Probe
- Scan Size: 10μm×10μm
- Scan Rate: 0.5Hz
- Pixel Size: 256 × 512