Limitations of Conventional 3D AFM
|
|
Flare Tip |
|
Tilted Step-in Tip |
Innovative XE-3DM Technology Overcomes the Challenges
|
|
High Resolution Access to Undercut and Sidewall
|
Image of Undercut Overhang: Metal Overhang Structure
|
|
3D View of High Resolution Sidewall Scan
|
Complete 3D Metrology of Sidewall |
|
Sidewall Roughness Measurement
|
|
Undercut & Sidewall Characterization
|
|
- Need to measure the sidewall roughness, angle and the width of bottom, middle, and top |
Challenges in Accessing Sidewall
|
|
Conventional AFM cannot get access to the sidewall, especially for overhang features |
|
Other methods, such as the flare tips, are insufficient in obtaining the high resolution details of the sidewall due to its dull tip. For a deeper overhang, the bottom width cannot be reached at all. |
For Undercut Characterization and Sidewall Metrology
Continuing the company’s impressive track record of developing optimized solutions, Park Systems introduces XE-3DM, an automatic AFM which revolutionizes the way trench, overhang, and undercut features are scanned and analyzed. The new XE-3DM also makes possible to image soft photoresist structures without deforming or damaging it.
|
Advanced Inline Automation Features |
Flat and very wide bottom portion of the tip (>100nm)