Probe Dynamics At Atomic Level In Situ Non Uniform Reaction Rates During Oxidation of Low-Chain
Speaker : Fang Xu Affiliation : Harvard University Region : US Year : 2019 Language : English Explore in situ non-uniform reaction rates during the oxidation of low-chain alcohols, focusing on methanol. Investigate surface structures and dynamics at the atomic level using scanning tunneling microscopy (STM). Gain insights into how surface structures influence heterogeneous catalysis, providing information for catalyst design and optimization.