Caracterizacion estructural y nanomecanica de materiales biologicos con microscopia de fuerza atomica y de superresolucion.

Speaker : Dr. Jorge Chanona Perez Affiliation : Nanotechnology, Instituto Politécnico Nacional, MEXICO Region : LatAm Year : 2021 Language : Spanish Explore research on nanomechanical properties of biological and food materials, including microstructure analysis using super-resolution microscopy. Learn about applications of atomic force microscopy (AFM) in characterizing materials, understanding mechanical properties, and studying changes during maturation and processing.