Tailoring Hydrogel Surfaces
Speaker : Prof. Nicholas D. Spencer Affiliation : ETH Zurich, Switzerland Region : Europe Year : 2021 Language : English Explore the intricacies of tailoring hydrogel surfaces to mimic cartilage properties using polymer brushes and gel characterization techniques like AFM. Understand the mold effect's role in modulating surface properties and friction in hydrogels.