Speaker : Ms. Chao Wen Affiliation : Soochow University, China Region : China Year : 2020 Language : English Explore the potential of calcium fluoride as a high-k dielectric for 2D electronics. Discover its compatibility with 2D materials like graphene and molybdenum disulfide, highlighting superior properties over traditional dielectrics like silicon dioxide.