HBN Polydimethylsiloxane Tape HexagonalBoronNitride domain_switching EPFL Grain nanobar HumanHair PhaseChange ForceVolume #EC SurfaceOxidation Electrode ring shape PVAC CrystalGrowing molecules Beads vertical_PFM Ceramic fluoroaalkane sputter thermal_conductivity Thermal LithiumNiobate CancerCell Lattice Nickel CrAu OxideLayer LowDensityPolyethylene ConductiveAFM India Global_Comm
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
HfO2 into Indium Tin Oxide Film
ITO film on 1% HfO2-doped Yttria-stabilized Zirconia (001) orientation grown by pulsed laser deposition. Surface segregation of HfO2 into ITO film.
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz))
- Scan Size: 10μm×10μm,5μm×5μm
- Scan Rate: 0.6Hz, 1Hz
- Pixel Size: 256 × 256, 256 x 256
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz))
- Scan Size: 10μm×10μm,5μm×5μm
- Scan Rate: 0.6Hz, 1Hz
- Pixel Size: 256 × 256, 256 x 256