contact CompactDisk PANI Permalloy Composite Potential NanoLithography pinpoint mode Terrace Phase neodymium_magnets Adhesive vertical_PFM PvdfFilm PetruPoni CBD Vac TyphimuriumBiofilm PvdfBead Lanthanum_aluminate FailureAnalysis exfoliate HexagonalBoronNitride Flake Sapphire MagneticForceMicroscopy MetalCompound PECurve Au111 AdhesionForce organic_polymer alkanes Gallium_Arsenide MultiferroicMaterials self-assembled_monolayer
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Formamidinium Lead Iodide FAPbI3 Perovskite Film
FAPbI3 is an organic-inorganic hybrid perovskite material for nowadays high efficiency perovskite solar cell.
Scanning Conditions
- System: NX10
- Scan Mode: Conductive AFM
- Cantilever: CDT-NCHR (k=80N/m, f=400kHz)
- Scan Size: 15μm×15μm
- Scan Rate: 0.5Hz
- Pixel Size: 512 × 256
- Scan Mode: Conductive AFM
- Cantilever: CDT-NCHR (k=80N/m, f=400kHz)
- Scan Size: 15μm×15μm
- Scan Rate: 0.5Hz
- Pixel Size: 512 × 256