temperature controller AFM Wang ScanningKelvinProbeMicroscopy Platinum Materials PtfeFilter ElectroChemical Optoelectonics Graphite Pinpoint fifber Inorganic_Compound Cobalt-dopedIronOxide UTEM AlkaneFilm ScanningThermalMicroscopy dielectric trench Piezoresponse Molybdenum SFAs GlassTemperature atomic_layer Cell molecular_beam I-VSpectroscopy PyroelectricDetector Dr.JurekSadowski StrontiumTitanate HDD ThermalProperties NUS_NNI_Nanocore Chemical_Vapor_Deposition Piezoelectric SAM UnivOfMaryland
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Fe Thin Films
MFM images of Fe thin films (80 nm) epitaxied on GaAs(001) and then implanted with N-atoms. Images reveal weak stripe domains at magnetic remanence.
Scanning Conditions
- System: NX10
- Scan Mode: MFM
- Cantilever: PPP-MFMR (k=2.8N/m, f=75kHz)
- Scan Size: 15μm×15μm,2μm×2μm
- Scan Rate: 0.5Hz, 1Hz
- Pixel Size: 512×512, 256×256
- Lift height: 50nm
- Scan Mode: MFM
- Cantilever: PPP-MFMR (k=2.8N/m, f=75kHz)
- Scan Size: 15μm×15μm,2μm×2μm
- Scan Rate: 0.5Hz, 1Hz
- Pixel Size: 512×512, 256×256
- Lift height: 50nm