cannabinoid PvdfFilm TungstenDeposition Chemical Vapor Deposition semifluorinated alkane Yeditepe Subhajjit VinylAlcohol Pvdf CeramicCapacitor Ferroelectric Sphere hard_disk SelfAssembly OpticalModulator CHRYSALIS_INC FuelCell PinpointNanomechanicalMode SiWafer Force-distance HumanHair vertical_PFM lift_mode Holes Mfm NeodymiumMagnets Transparent Nanofiber Moire exfoliate MetalCompound EPFL AM_KPFM layers Optoelectonics
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Christmas Ball Lithography on Si
Create oxidation layers on bare Si surface using bias mode of lithography.
Scanning Conditions
- System: NX10
- Scan Mode: Lithography
- Cantilever: AD-40-SS (k=40N/m, f=200kHz)
- Scan Size: 40μm×40μm
- Scan Rate: 0.5Hz
- Pixel Size: 1024 × 1024
- Tip Bias: -10V for patterened area
- Scan Mode: Lithography
- Cantilever: AD-40-SS (k=40N/m, f=200kHz)
- Scan Size: 40μm×40μm
- Scan Rate: 0.5Hz
- Pixel Size: 1024 × 1024
- Tip Bias: -10V for patterened area