MESA structure Strontium Inorganic_Compound StyreneBeads Electical&Electronics GaAs Cancer Roughness rubber non_contact ring shape BiVO4 Change FrequencyModulation Microchannel NUS_NNI_Nanocore SurfaceOxidation Butterfly amplitude_modulation Piezoelectric Spain Fet thermal_conductivity self_assembly LiIonBattery Optoelectronic CNT conductive Adhesive Austenite Chemical Vapor Deposition Conductivity Plug heterojunctions AAO
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Block Copolymer Embedded in Rubber
Block copolymer embedded in rubber cross-section.
Scanning Conditions
- System: NX20
- Scan Mode: Pinpoint
- Cantilever: NSC36Cr-Au B (k=2N/m, f=130kHz)
- Scan Size: 1μm×1μm
- Scan Rate: 0.29Hz
- Pixel Size: 256 × 256
- Scan Mode: Pinpoint
- Cantilever: NSC36Cr-Au B (k=2N/m, f=130kHz)
- Scan Size: 1μm×1μm
- Scan Rate: 0.29Hz
- Pixel Size: 256 × 256