Spain Pattern Wonseok light_emission StyreneBeads LiftMode Temperature KAIST Sapphire Thermal PVAC IcelandSpar Biofilm Tape margarine Gallium_Arsenide BCZT YttriaStabilizedZirconia molecules PpLdpe SicMosfet piezoelectric force microscopy solar_cell IRDetector Logo MagneticForce nanomechanical Heat ScanningSpreadingResistanceMicroscopy AdhesionEnergy temp_control SrO strontiu_titanate mechanical property TungstenThinFilmDeposition
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
PS/LPDE
Spincast layer of PS/LDPE blend on Si. Signal change by thermal conductivity difference.
Scanning Conditions
- System: NX10
- Scan Mode: SThM
- Cantilever: NanoThermal Probe
- Scan Size: 10μm×10μm
- Scan Rate: 0.5Hz
- Pixel Size: 256 × 512
- Scan Mode: SThM
- Cantilever: NanoThermal Probe
- Scan Size: 10μm×10μm
- Scan Rate: 0.5Hz
- Pixel Size: 256 × 512