Vinylpyridine Protein Piranha Tin sulfide AEAPDES ThermalConductivity hard_disk EPFL frequency_modulation SelfAssembly INSPParis Strontium Moire temperature_control BloodCell Polydimethylsiloxane EFM piezoelectric force microscopy block_copolymer fifber Polyurethane Cell Collagen FrictionalForce Polystyrene graphene_hybrid dielectric trench GlassTemp lift_mode Tapping Galfenol Heat Aggregated_molecules CancerCell molecular_self_assembly
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Plate-shaped DNA origami
Scanning Conditions
- System : FX40
- Scan Mode: Tapping in Liquid
- Scan Rate : 1Hz
- Scan Size : 250nm×250nm
- Pixel Size : 512×256
- Cantilever : USC-F0.3-k0.3 (k=0.3N/m, f=300kHz)