LiNbO3 BTO UnivMaryland LiquidImaging AtomicSteps Etch FailureAnalysis Electical&Electronics LeakageCurrent CP-AFM Nickel Magnetic Force Microscopy DeoxyribonucleicAcid Ito C36H74 margarine UTEM Device cannabidiol PUR ScanningTunnelingMicroscopy AM-KPFM LogAmplifier LiftMode graphene_hybrid ElectroChemical PolyimideFilm Co/Cr/Pt TappingMode HexacontaneFilm Resistance F14H20 multi_layer LDPE CrAu
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Diamond with plated / gold nickel
Scanning Conditions
- System : NX20
- Scan Mode: Non-contact
- Scan Rate : 0.49 Hz for 30μm2, 4μm2 / 0.6 Hz for 2.25m2
- Scan Size : 30μm2, 2.25μm2, 4μm2
- Pixel Size : All 256×256
- Cantilever : AD-2.8-AS (k=2.8N/m, f=75kHz)