ContactMode Piezo LateralForceMicroscopy Leakage Copolymer Organic 2d_materials membrane CuFoil Force-distance GalliumPhosphide dichalcogenide pinpoint mode ito_film Magnetic PVAP3HT ULCA SICM BloodCell epitaxy Styrene solar_cell Ca10(PO4)6(OH)2 Zagreb TemperatureControllerAFM Nickel Bismuth flakes Topography AmplitudeModulation KAIST atomic_layer Bmp NUS_NNI_Nanocore AM-KPFM
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
MoSi₂ Hard defect repair
Scanning Conditions
- System : NX-Mask
- Scan Mode: Non-contact for imaging Sweep for repairing
- Scan Rate : 0.3 Hz
- Scan Size : 6μm, 0.5μm×1μm
- Pixel Size : 512×64 for 6μm2, 512×34 for 0.5μm×1μm