AmplitudeModulation SSRM #EC PvdfBead TCS Al2O3 Phthalocyanine ScanningThermalMicroscopy Topography HiVacuum PolymerPatterns mechanical_property Layer PatternedSapphireSubstrat Pores HanyangUniv TriGlycineSulphate Led suspended_graphene KevlarFiber Adhesion Temasek_Lab kelvin probe force microscopy LifeScience IRDetector Korea PtfeFilter Dimethicone Thermoplastic_polyurethane Heat mfm_amplitude Flake Polydimethylsiloxane Sidewall ForceMapping
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Suspended silicon nitride membrance
Scanning Conditions
- System : NX20
- Scan Mode: Tapping
- Scan Rate : 0.2 Hz
- Scan Size : 75μm×75μm
- Pixel Size : 256×256
- Cantilever : TESPA-V2 (k=37N/m, f=320kHz)