Mobile gallium_nitride Tin sulfide SoftSample AmplitudeModulation Device DentalProsthesis Iron Annealed Mapping Magnets Adhesion Liquid Co/Cr/Pt LDPE NiFe StyreneBeads AnodizedAluminumOxide Silicon dielectric_trench GlassTemperature align BFO chemical_compound Glass Nanofiber Inorganic Ceramic HDD temperature controller AFM Scanning_Thermal_Microscopy OpticalElement FAFailureAnlaysis PhaseChange CrAu
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
hBN-few layer Graphene
Scanning Conditions
- System : NX10
- Sample bias: 1.75 V
- Scan Mode: C-AFM
- Scan Rate : ALL 0.5Hz
- Scan Size : 200nm×200nm
- Pixel Size : 2048×2048
- Cantilever : AD-2.8-AS (k=2.8N/m, f=75kHz)