PpLdpe Foil ShenYang Polypropylene FrequencyModulation CuParticle PolymerPatterns margarine alkanes LithiumNiobate Yeditepe TemperatureControllerStage UnivOfMaryland Chemical_Vapor_Deposition Polyurethane Reduction LowDensityPolyethylene electrospinning ItoGlass Sphere StainlessSteel Biology FrictionForce Current Deposition Spain DeoxyribonucleicAcid PiezoelectricForceMicroscopy fluoroalkane Water CrossSection Cancer Polyaniline FM_KPFM Tungsten_disulfide
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Galfenol (Alloy of iron and gallium)
Scanning Conditions
- System: XE15
- Scan Mode: MFM
- Cantilever: MFMR (k=2.8N/m, f=70kHz)
- Scan Size: 40μm×40μm
- Scan Rate: 0.5Hz
- Pixel: 256×256
- MFM Lift height: 50nm