MESA structure rubber non_contact Mechanical strontiu_titanate Tapping NUSNNI Genetic ContactModeDots NCM polymeric_arrays Boundary Lateral Pore AnodizedAluminumOxide Barium_titanate Ram MembraneFilter Semiconductor 2d_materials conductive FM_SKPM Strontium TipBiasMode DOE Spincast CompactDisk CeramicCapacitor cross section Gallium_Arsenide Platinum Sio2 AM_KPFM Adhesive Glass
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
STO(SrTiO3), Annealed LAO(LaAlO3)
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 2μm×2μm, 5μm×5μm
- Scan Rate: 0.8Hz, .9Hz
- Pixel: 512×512, 256×256