PolymerBlend Sphere GaAs Chloroform amplitude_modulation AtomicLayer InorganicCompound Sio2 kelvin probe force microscopy IIT-chennai IcelandSpar Gong polyvinyl acetate Alloy PVA LifeScience nanobar Magnetic Ferroelectric ScanningIon-ConductanceMicroscopy LMF Piezoresponse PatternedSapphireSubstrat MLCC Growing NeodymiumMagnets STM Polydimethylsiloxane Optic CalciumHydroxyapatite LiBattery heterojunctions Chemical Vapor Deposition TemperatureControllerStage TemperatureControlledAFM
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Polymer patterns on Si (1/2)
Scanning Conditions
- System: NX10
- Scan Mode: KPFM
- Cantilever: NSC36Cr-Au (k=1N/m, f=90kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 0.2Hz
- Pixel: 512×256