ScanningTunnelingMicroscopy MagneticArray Polarization Mobile MagneticForceMicroscopy LightEmiting MagneticForce hetero_structure organic_polymer lift_mode BiFeO3 Styrene Device Laser Holes Pores Resistance FrictionalForceMicroscopy ForceDistanceSpectroscopy Switching Implant mfm_amplitude temperature controller AFM Leakage NiFe INSP HanyangUniv MembraneFilter molecular_self_assembly AAO Bacterium TungstenDeposition fluoroalkane DomainSwitching MeltingPoint
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
BN thin film on Si
Scanning Conditions
- System: NX10
- Scan Mode:SThM
- Cantilever: Nanothermal probe
- Scan Size: 25μm×25μm, 5μm×5μm
- Scan Rate:0.3Hz, 0.5Hz
- Pixel: 256×256, 256×256
- Scan Mode:SThM
- Cantilever: Nanothermal probe
- Scan Size: 25μm×25μm, 5μm×5μm
- Scan Rate:0.3Hz, 0.5Hz
- Pixel: 256×256, 256×256