Park AFM Imaging Modes

True Non-Contact™ Mode

non-contact-mode

Consistently produces high resolution and accurate data while maintaining the integrity of sample.

The True Non-Contact mode preserves tip sharpness and sample surface, and you can get more accurate results. In the True Non-Contact mode, a piezoelectric modulator vibrates a cantilever at small amplitude and a fixed frequency near the resonant frequency of the cantilever. As the tip is brought closer to the sample, the van der Waals attractive force between tip and sample changes the amplitude and the phase of the cantilever’s vibration. These changes are monitored by the patented Z-servo feedback system of the Park AFMs, which maintains a tip-surface distance of just a few nanometers without damaging the sample surface or the tip end.

Read More

 

Nano-arrayed-particles

Nano-arrayed particles
Scan size: 1μm, 250nm, 120nm
Using Probe: AR5T-NCHR
Imaged on a Park NX10 using Non-contact Mode.

Contact Mode

contact-mode

The simplest scanning method to image the surface

The contact mode is the simplest way to acquire the sample topography. The topography signal comes from the Z scanner position, which maintains the deflection of the cantilever constant on the sample surface.

Read More

 

contact_pmg-crystal

[Initial Topography]   /   [Topography change After 30min]

PMG Crystal in glyphosate solution
Scan size: 2μm
Using Probe: Biolever mini
Imaged on a Park NX10 using contact mode in liquid.

Tapping Mode

tapping-mode

In this alternative technique to non-contact mode, the cantilever again oscillates just above the surface, but at a much higher amplitude of oscillation. The bigger oscillation makes the deflection signal large enough for the control circuit, and hence an easier control for topography feedback. It produces modest AFM results but blunts the tip’s sharpness at a higher rate, ultimately speeding up the loss of its imaging resolution.

Read More

 

phase-imaging-crystal-facetts

[Topography]   /   [Phase]
Phase image of Crystal Facetts, collected simultaneously.

Crystal Facetts
Scan size: 10 µm
Using Probe: AC160TS
Imaged on a Park NX10 using Tapping mode.