PZT nanotubes on Nb-STO

PZT nanotubes on Nb-STO 2

Scanning Conditions

- System: NX20
- Scan Mode: NCM, Piezo response curve
- Cantilever: NCHR, ContscPt
- Scan Size: 2μm×2μm, 2μm×2μm
- Scan Rate: 0.3Hz, 0.3Hz
- Pixel: 512×512, 512×512