Li stripping-plating on Li surface
The Li surface was observed using Electrochemical Atomic Force Microscopy (EC-AFM) during the stripping–plating process.
Sequential height images show the surface evolution from the fresh Li surface to after 5 minutes of stripping and after 5 minutes of plating, visualizing nanoscale changes induced by electrochemical cycling.
Scanning Conditions
- System: NX12
- Scan Mode: Electrochemical AFM
- Scan Rate: 0.15 Hz
- Scan Size: 30 µm × 30 µm
- Pixel Size: 256 × 256 pixels
- EC: Li metal (Working electrode), Li metal (Reference electrode), Li (Counter electrode), 1M LiTFSI in TEGDME (Electrolyte)