Metrology - Non-Contact Mode
With the increasing shrinkage of device sizes, the characterization of thin films and their structures becomes critical to optimizing the resulting device at the end of line. For example, CD etch variation is directly related to the angle of the resist profile. In the images below, the strength of the Park AFM instruments to measure wall angles is demonstrated.
![]()
The etch angle between Silicon (111) and (100) is 54.7 degrees. The measured etch angle of the silicon structure is approximately 54.6 degrees.
![]()
The measured angle of the etched silicon holes shows a consistent angle on all sides. Very low angle measurements, such as these, can be measured with confidence using the high flatness scanner of the Park AFM.
Sample:
- Top: Etched Si (111) with etch angle 54.7 degrees
- Bottom: Etched Si Structure
Image Conditions:
- True Non-Contact Mode
System Requirement:
- Closed-loop AFM System
- Decoupled XY and Z scanners
- High Flatness XY scanner
The Benefits
The key factors effecting angle measurement are:
- the orthogonality of the
scanners used to image
the sample
- half cone angle of
cantilever tip
- system drift
The decoupled XY and Z scanner design minimizes artifacts resulting in enhanced wall angle measurement repeatability.