Speaker : Kim McKelvey Affiliation : Trinity College Dublin, Ireland Region : Europe Year : 2019 Language : English The lecture explores the correlation between structure and electrochemical activity, focusing on CO2 reduction at grain boundaries. By studying nanoscale relations, researchers can design devices for more efficient CO2 reduction. The integration of scanning electrochemical microscopy (SECM) with AFM allows for simultaneous analysis of activity and structure, facilitating rational device design.