Speaker : Dr. Subhrajit Mukherjee Affiliation : 以色列理工学院 (Technion-Israel Institute of Technology) Region : China Year : 2022 Language : English The search of ultrathin and robust ferroelectrics leads to few promising two-dimensional (2D) materials. Among those, α-phase In2Se3 has drawn a special attention owing to the existence of intercoupled in-plane (IP) and out-of-plane (OOP) ferroelectricity in monolayer form, which makes it a potential candidate for emerging artificial intelligence, information processing and memory applications[1]. Mostly, Piezoelectric force microscopy (PFM) is used to identify the ferroelectricity in 2D materials, where the polarization direction changes under the applied electric field is reflected as phase contrast[2]. However, the contact-mode PFM causes layer damages, in particular if any steps or roughness are present in the topography. Therefore, an alternative non-contact mode characterization technique, like Kelvin-probe force microscopy (KPFM), can be useful to identify the electric field direction in non-destructive way[1]. To provide a proof-of-concept demonstration in device level, we performed KPFM measurements on a ferroelectric-semiconductor field-effect transistors (FeS-FET) under operational conditions[3-5]. Here, we showed a repeatable and reversible IP ferroelectric switching across the device channel, realized by a vertical electric field applied through gate electrode, which also established the inherent orthogonal dipole coupling[3]. Moreover, the interfacial band formations between all the dissimilar materials (including metal electrodes), respective CB and VB offsets, junctions type, effect of ferroelectric dipoles, are deduced via KPFM for coplanar In2Se3-In2O3 heterostructure FETs[4-5]. In conclusion, KPFM is an effective non-destructive method with high spatial resolution over domain orientation, for fast detection of 2D ferroelectricity, which becomes beneficial for research and device innovation.
Electronic properties of 2D ferroelectric layer based FET's using Kelvin - probe force microscopy
×