Enriching your AFM data: KPFM high resolution imaging of ferroelectric domains with automated AFM
SPEAKERS
  • James Kerfoot
    Park Systems UK Ltd, Nottingham, United Kingdom
Authors
James Kerfoot

Check out all webinars from the Empowering AFM Imaging series here.

The formation of layered materials heterostructures affords a unique degree of freedom in material design: the inter-layer twist angle. By modifying the twist angle between two crystalline materials, the registry of atoms may be continuously modified on length scales on the order of 0.1 to 1000 nm, supporting a host of exotic phenomena such as Wigner crystals [1], flat bands [2] and superconductivity [3]. Among all state-of-the-art characterisation techniques, scanning probe microscopy is particularly powerful tool in the study of such samples since it can be used to measure both atomic registry of such layered materials heterostructures and their associated functional properties at sub-nanometre length scales. One such property to have received extensive recent attention is the formation of ferroelectric domains in parallel stacked hBN [4-6]. In this webinar, we discuss the characterisation of ferroelectric bilayer hBN using scanning probe microscopy on the Park FX40 Automatic AFM. In the first part of the demo, an overview of formation of ferroelectric hBN samples and the operating principles of Kelvin probe force microscopy (KPFM) will be given. We will then provide a whistle-stop tour of the factors limiting the resolution and accuracy of contact potential difference (CPD) measurements in KPFM, and how these are better minimised using sideband KPFM. In the second part of this webinar, a live demonstration of KPFM carried out on ferroelectric bilayer-hBN on the Park FX40 system will take place. We will first exhibit the unique automation available on the Park FX40 system, enabling rapid preparation of AFM experiments. We will then proceed to discuss the setup of both electrostatic force microscopy (EFM) and frequency modulated sideband KPFM in order to map the work function of layered materials and ferroelectric domains in twisted bilayer hBN.

In addition to showcasing the unique automation in both the setup and execution of AFM experiments provided by the new FX40 AFM, we demonstrate a workflow to characterise the morphology and strength of ferroelectric domains in layered materials with state-of-the-art spatial resolution and electrical sensitivity. This work will be taken forward in further webinars where we address electron tunnelling from graphene through ferroelectric hBN on the nanometre scale which can be used to deterministically switch domains and induce asymmetry in point current-voltage characteristics of such samples, with applications both to memristive devices and tunnel diodes capable of offering increased logic per chip.

[1] H. Li et al. Nature 597, 650–654 (2021).
[2] E. Li et al. Nat Commun 12, 5601 (2021).
[3] Y. Cao et al. Nature 556, 43–50 (2018).
[4] C. R. Woods et al. Nat Commun. 12, 347 (2021).
[5] K. Yasuda et al. Science 372, 6549 1458 (2021)
[6] M. Vizner Stern et al. Science 372, 6549, 1462, (2021).